Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 6401 Phenolic, Briquette, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Glass Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 6401 Phenolic, Briquette, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.750 g/cc
0.0271 lb/in³
ASTM D1895
Density 1.76 g/cc
0.0636 lb/in³
ASTM D792
Water Absorption 0.066 %
0.066 %
ASTM D570
Linear Mold Shrinkage 0.00086 cm/cm
0.00086 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 99
99
ASTM D785
Tensile Strength, Ultimate 108 MPa
15700 psi
ASTM D638
Elongation at Break 0.84 %
0.84 %
ASTM D638
Tensile Modulus 15.8 GPa
2290 ksi
ASTM D638
Flexural Strength 182 MPa
26400 psi
ASTM D790
Flexural Modulus 16.2 GPa
2350 ksi
ASTM D790
Compressive Strength 282 MPa
40900 psi
ASTM D695
Izod Impact, Notched 0.440 J/cm
0.824 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.440 J/cm²
2.09 ft-lb/in²
ASTM D256
Impact 260
260
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 228 °C
442 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 280 °C
536 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Shrinkage 0.040 %
0.040 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 5.20e+11 ohm-cm
5.20e+11 ohm-cm
ASTM D247
Dielectric Constant 5.6
5.6
ASTM D150
Dielectric Strength 8.60 kV/mm
218 kV/in
Step by Step; ASTM D149
11.7 kV/mm
297 kV/in
Short Time; ASTM D149
Dissipation Factor 0.031
0.031
ASTM D150
Arc Resistance 102 sec
102 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved