Maximum Service Temperature, Air 97.2 °C
207 °F
Heat Distortion, Annealed; ASTM D648
Total 680 Polystyrene  (discontinued **)
Polystyrene 680 is a medium impact polystyrene developed for the foam extrusion and laminate markets. This polymers impact qualities in conjunction with its high flexural strength allow 680 to be ex..
Maximum Service Temperature, Air 97.0 - 110 °C
207 - 230 °F
Softening Range
Huntsman Araldite GT 7074 Bisphenol A Epoxy Solid Resin
Weight per Epoxide (EEW, g/eq) 935 to 1175. Max color is 2.Comments/Applications: Unmodified bis A "Type 4+" epoxy. Medium melt viscosity epoxy for thick film powder coatings. Outstanding adhesio..
Maximum Service Temperature, Air 97.0 °C
207 °F
Heat Distortion Temp
Hannam Chemical Hanalac H-2938 ABS
Maximum Service Temperature, Air 97.2 °C
207 °F
Heat Distortion, Annealed; ASTM D648
Total PSC 523 Polystyrene
Polystyrene 523 is a high flow, high heat crystal. Specially designed for foam applications it has a very narrow molecular weight distribution. Performance in extruded loose fill foam is excellent d..
Maximum Service Temperature, Air 97.0 °C
207 °F
for 50% loss of tensile strength after 5000hr
BASF Ultramid® B3S BK00464 PA6 (Conditioned)
Description: Easy flowing, finely crystalline injection-molding grade for very fast processing. Uses include thin-walled technical parts (eg. housings, fittings, grips, small parts and fixing clamps..
Maximum Service Temperature, Air 97.0 °C
207 °F
for 50% loss of tensile strength after 5,000 hr
BASF Ultramid® B3S BK00464 PA6 (Dry)
Ultramid B3S BK00464 is an easy flowing, pigmented black, finely crystalline injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500.
Maximum Service Temperature, Air 97.0 °C
207 °F
for 50% loss of tensile strength after 5,000 hr
BASF Ultramid® B3S HP PA6 (Conditioned)
Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing
Maximum Service Temperature, Air 97.0 °C
207 °F
for 50% loss of tensile strength after 5,000 hr
BASF Ultramid® B3S HP PA6 (Dry)