Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hannam Chemical Hanalac H-2938 ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Hannam Chemical
Trade Name Hanalac
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hannam Chemical Hanalac H-2938 ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Melt Flow 2.3 g/10 min
2.3 g/10 min
ASTM D1238G
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength, Ultimate 48.0 MPa
6960 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Yield Strength 68.6 MPa
9950 psi
ASTM D790
Flexural Modulus 2.26 GPa
328 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 97.0 °C
207 °F
Heat Distortion Temp
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C
207 °F
ASTM D648
Vicat Softening Point 115 °C
239 °F
ASTM D1525
Users viewing this material also viewed the following: