Thermal Properties Metric English Comments
Maximum Service Temperature, Air 128 - 280 °C
262 - 536 °F
Average value: 162 °C Grade Count:5
Overview of materials for Nylon 46, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Maximum Service Temperature, Air 128 °C
262 °F
5000 hours Thermal Index; IEC 60216/ISO 527-1/-2
DSM Stanyl® TE300 PA46
Heat Stabilized
Copyright © lookpolymers.com All Rights Reserved