Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 82.2 - 121 °C | 180 - 250 °F | Average value: 118 °C Grade Count:45 |
Overview of materials for Methacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropri.. |