Polymer Property : Maximum Service Temperature, Air = -67.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air -55.0 - 150 °C
-67.0 - 302 °F
SMACSIL®
SMAC SMACDISK® 1114S Damping Material
Specifications - Shock & vibration insulation for:Hard diskLow frequency dampingVehicular electronicsRequiring vibration isolationInformation provided by SMAC MontBlac Groupe Technologies
Maximum Service Temperature, Air -55.0 - 150 °C
-67.0 - 302 °F
SMACSIL®
SMAC SMACMOUNT® 1195S Damping Material
Specifications - Shock & vibration insulation for:Embedded electronicTrays & racks systemsAdvantages:No special tools requiredHigh damping isolatorsSmall SizeInformation provided by SMAC MontBlac Gr..
Maximum Service Temperature, Air -55.0 - 150 °C
-67.0 - 302 °F
SMACSIL®
SMAC SMACMOUNT® 2528S Damping Material
Specifications - Shock & vibration insulation for:Aircraft avionics components & subassembliesMissile electronicsVehicular electronics requiring vibration isolationAdvantages :Bushing style mountCou..
Maximum Service Temperature, Air -55.0 - 150 °C
-67.0 - 302 °F
SMAC SMACMOUNT® 2112S Damping Material
Specifications - Shock & vibration insulation for:Aircraft avionics components & subassembliesMissile electronicsVehicular electronics requiring vibration isolationAdvantages :Bushing style mountCou..
Maximum Service Temperature, Air -55.0 - 150 °C
-67.0 - 302 °F
SMAC SMACMOUNT® 2132S Damping Material
Specifications - Shock & vibration insulation for:Airborne components and electronic packagesMissile systems and electronicsAirborne avionics unitsGyro, optic, & laser components and assembliesAdvan..
Maximum Service Temperature, Air -55.0 - 150 °C
-67.0 - 302 °F
SMAC SMACMOUNT® 2150S Damping Material
Specifications - Shock & vibration insulation for:Electronic components and subassemblies (Disk drive, Guidance system, radar…)High frequency vibration isolationStructural element vibration bre..
Maximum Service Temperature, Air -55.0 - 150 °C
-67.0 - 302 °F
SMAC SMACMOUNT® 2151S Damping Material
Specifications - Shock & vibration insulation for:Electronic components and subassemblies (Disk drive, Guidance system, radar…)High frequency vibration isolationStructural element vibration bre..
Maximum Service Temperature, Air -55.0 - 150 °C
-67.0 - 302 °F
SMAC SMACMOUNT® 2527S Damping Material
Specifications - Shock & vibration insulation for:Aircraft avionics components & subassembliesAirborn electronicsAdvantages:Light weightSave spaceDouble the stiffness and countersink using 2 mounts ..