SMAC SMACMOUNT® 2527S Damping Material

Category Other Engineering Material
Manufacturer SMAC
Trade Name SMACMOUNT®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SMAC SMACMOUNT® 2527S Damping Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Specifications - Shock & vibration insulation for:Aircraft avionics components & subassembliesAirborn electronicsAdvantages:Light weightSave spaceDouble the stiffness and countersink using 2 mounts back to backInformation provided by SMAC MontBlac Groupe Technologies
Thermal Properties Metric English Comments
Maximum Service Temperature, Air -55.0 - 150 °C
-67.0 - 302 °F
Descriptive Properties Value Comments
Axial/Radial frequency ratio 0.7
Frequency > 25 Hz
Load <2 kg
120 N
2 mm, Radial
15 N
0.5 mm, Axial
15 N
0.5 mm, Raidal
30 N
1 mm, Radial
30 N
1.5 mm, Axial
60 N
3 mm, Axial
Materials SMACSIL®
Maximum axial deflection 4 mm
Metal parts Aluminum
Q 4
Transmissibility at resonance <4
0.7
100 Hz, Axial
1
60 Hz, Axial
1
20 Hz, Axial
3
33 Hz, Axial
Weight 5.4 g