Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SMAC SMACMOUNT® 1195S Damping Material

Category Other Engineering Material
Manufacturer SMAC
Trade Name SMACMOUNT®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SMAC SMACMOUNT® 1195S Damping Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Specifications - Shock & vibration insulation for:Embedded electronicTrays & racks systemsAdvantages:No special tools requiredHigh damping isolatorsSmall SizeInformation provided by SMAC MontBlac Groupe Technologies
Thermal Properties Metric English Comments
Maximum Service Temperature, Air -30.0 - 80.0 °C
-22.0 - 176 °F
SMACTANE®
-55.0 - 150 °C
-67.0 - 302 °F
SMACSIL®
Descriptive Properties Value Comments
Frequency 100-140 Hz
Load 2.2 - 6.6 lbs
Materials SMACSIL®
SMACTANE®
Metal parts Stainless steel
Overall size 13 mm
ø ext.
27 mm
Height
Transmissibility at resonance <2.5
SMACTANE®
<4
SMACSIL®
Weight 2.5 g