Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.44 W/m-K @Temperature 80.0 °C |
9.99 BTU-in/hr-ft²-°F @Temperature 176 °F |
ASTM C518 |
Rogers Corporation RT/duroid® 6035HTC Ceramic Filled PTFE Composite, High Power RF and Microwave Features & Benefits:High thermal conductivity - Improved dielectric heat dissipation, enabling lower operating temperatures for high power applicationsLow loss tangent - Excellent high frequency per.. |
|||
Thermal Conductivity | 1.44 W/m-K | 9.99 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® E3035T-2 Electrically Conductive Epoxy Product Description: EPO-TEK® E3035T-2 is a single component, silver-filled epoxy for semiconductor die attach, as well as SMD attach on hybrid circuits.Advantages & Application Notes: This epoxy c.. |