Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.37 W/m-K | 9.51 BTU-in/hr-ft²-°F | |
Sharadaa Ceramics REFINSUL 4 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Thermal Conductivity | 1.37 W/m-K | 9.51 BTU-in/hr-ft²-°F | |
Trelleborg Emerson & Cuming Stycast® 2762/17M-1 Two-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Thermal Conductivity | 1.37 W/m-K | 9.51 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® E4110 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E4110 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although other.. |