Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 12.22 W/m-K @Temperature 23.0 °C |
84.81 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
|
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 20% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |
|||
Thermal Conductivity | 12.22 W/m-K @Temperature 23.0 °C |
84.81 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
|
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 10% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |
|||
Thermal Conductivity | 12.22 W/m-K @Temperature 23.0 °C |
84.81 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
|
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 0% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |