Thermal Conductivity 11.9 W/m-K
82.6 BTU-in/hr-ft²-°F
RT
Outokumpu 4841 High Temperature Austenitic Stainless Steel
Variant of 1.4845 with an increased silicon content which enhances the steel's resistance to oxidation/corrosion but has also made it more susceptible to embrittlement.Applications: Heat and creep r..
Thermal Conductivity 11.9 W/m-K
82.6 BTU-in/hr-ft²-°F
RT
Outokumpu 4845 High Temperature Austenitic Stainless Steel
Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o..
Thermal Conductivity 11.9 W/m-K
82.6 BTU-in/hr-ft²-°F
DIN EN 821-2 / ASTM-C408
CeramTec 192/193 Titania
192/193 is an excellent material for textile and other structural applications, where superior surface finishes are required with high chemical resistance. 193 is identical except it is metallic gra..