Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 4.69 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.50 - 4.69 W/m-K

@Temperature 50.0 - 50.0 °C
10.4 - 32.5 BTU-in/hr-ft²-°F

@Temperature 122 - 122 °F
Average value: 1.94 W/m-K Grade Count:4
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Thermal Conductivity 1.50 - 4.69 W/m-K

@Pressure 30.0 - 30.0 MPa
10.4 - 32.5 BTU-in/hr-ft²-°F

@Pressure 4350 - 4350 psi
Average value: 1.94 W/m-K Grade Count:4
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Thermal Conductivity 1.50 - 4.69 W/m-K

@Temperature 50.0 - 50.0 °C
10.4 - 32.5 BTU-in/hr-ft²-°F

@Temperature 122 - 122 °F
Average value: 2.08 W/m-K Grade Count:4
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..
Thermal Conductivity 1.50 - 4.69 W/m-K

@Pressure 30.0 - 30.0 MPa
10.4 - 32.5 BTU-in/hr-ft²-°F

@Pressure 4350 - 4350 psi
Average value: 2.08 W/m-K Grade Count:4
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..