Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.50 - 4.69 W/m-K @Temperature 50.0 - 50.0 °C |
10.4 - 32.5 BTU-in/hr-ft²-°F @Temperature 122 - 122 °F |
Average value: 1.94 W/m-K Grade Count:4 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Thermal Conductivity | 1.50 - 4.69 W/m-K @Pressure 30.0 - 30.0 MPa |
10.4 - 32.5 BTU-in/hr-ft²-°F @Pressure 4350 - 4350 psi |
Average value: 1.94 W/m-K Grade Count:4 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Thermal Conductivity | 1.50 - 4.69 W/m-K @Temperature 50.0 - 50.0 °C |
10.4 - 32.5 BTU-in/hr-ft²-°F @Temperature 122 - 122 °F |
Average value: 2.08 W/m-K Grade Count:4 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Thermal Conductivity | 1.50 - 4.69 W/m-K @Pressure 30.0 - 30.0 MPa |
10.4 - 32.5 BTU-in/hr-ft²-°F @Pressure 4350 - 4350 psi |
Average value: 2.08 W/m-K Grade Count:4 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |