Polymer Property : Thermal Conductivity = 4.03 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.500 - 0.580 W/m-K

@Temperature 100 - 100 °C
3.47 - 4.03 BTU-in/hr-ft²-°F

@Temperature 212 - 212 °F
Average value: 0.540 W/m-K Grade Count:3
Overview of materials for Phenolic, Novolac, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o..
Thermal Conductivity 0.540 - 0.580 W/m-K
3.75 - 4.03 BTU-in/hr-ft²-°F
Average value: 0.560 W/m-K Grade Count:3
Overview of materials for Phenolic, Novolac, Cellulose Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu..
Thermal Conductivity 0.580 - 0.580 W/m-K

@Temperature 100 - 100 °C
4.03 - 4.03 BTU-in/hr-ft²-°F

@Temperature 212 - 212 °F
Average value: 0.580 W/m-K Grade Count:1
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum ..