Polymer Property : Thermal Conductivity = 28.7 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 28.7 W/m-K

@Temperature 1000 °C
199 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes HR-160® alloy plate, aged 1000 hours at 649°C (1200°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 28.7 W/m-K

@Temperature 1000 °C
199 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes HR-160® alloy plate, aged 4000 hours at 649°C (1200°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 28.7 W/m-K

@Temperature 1000 °C
199 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes HR-160® alloy, annealed plate
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 28.7 W/m-K

@Temperature 1000 °C
199 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes HR-160® alloy, plate, aged 1000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 28.7 W/m-K

@Temperature 1000 °C
199 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes HR-160® alloy, plate, aged 1000 hours at 871°C (1600°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 28.7 W/m-K

@Temperature 1000 °C
199 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes HR-160® alloy, plate, aged 4000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 28.7 W/m-K

@Temperature 1000 °C
199 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes HR-160® alloy, plate, aged 4000 hours at 871°C (1600°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 28.7 W/m-K

@Temperature 1000 °C
199 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes HR-160® alloy, plate, aged 8000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 28.7 W/m-K

@Temperature 1000 °C
199 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes HR-160® alloy, plate, aged 8000 hours at 871°C (1600°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Thermal Conductivity 28.7 W/m-K

@Temperature 1000 °C
199 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..