Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 3.46 W/m-K | 24.0 BTU-in/hr-ft²-°F | |
SGL Carbon Group Ridurid® V 1017 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Thermal Conductivity | 3.46 W/m-K | 24.0 BTU-in/hr-ft²-°F | |
SGL Carbon Group Ridurid® V 1352 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Thermal Conductivity | 3.46 W/m-K | 24.0 BTU-in/hr-ft²-°F | |
SGL Carbon Group Ridurid® V 1640 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Thermal Conductivity | 3.46 W/m-K @Temperature 93.3 °C |
24.0 BTU-in/hr-ft²-°F @Temperature 200 °F |
|
Crucible Steel CSM® 2 Mold Steel, AISI P20 CSM 2 is a prehardened, general purpose mold steel suitable for production of machined or EDM’d plastic mold and zinc die casting die components. CSM 2 is supplied prehardened at two hardnesses: re.. |
|||
Thermal Conductivity | 3.46 W/m-K @Temperature 93.3 °C |
24.0 BTU-in/hr-ft²-°F @Temperature 200 °F |
|
Crucible Steel Nitriding #135 Modified Steel, AISI 4140 Modified Nitriding #135 steel is a modification of AISI 4140 specifically designed to be nitrided for high surface hardness and abrasion resistance.Information provided by Crucible Industries |
|||
Thermal Conductivity | 3.46 W/m-K | 24.0 BTU-in/hr-ft²-°F | |
Cymat A35620SC 030SS Stabilized Aluminum Foam Description: Cymat A35620SC 030SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.3 g/cm3. The mechanical properties of SAF make it .. |