Crucible Steel CSM® 2 Mold Steel, AISI P20

Category Metal , Ferrous Metal , Tool Steel
Manufacturer Crucible Steel
Trade Name CSM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Steel CSM® 2 Mold Steel, AISI P20.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CSM 2 is a prehardened, general purpose mold steel suitable for production of machined or EDM’d plastic mold and zinc die casting die components. CSM 2 is supplied prehardened at two hardnesses: regular at about 300 BHN and high hard at about 340 BHN.Information provided by Crucible Industries
Physical Properties Metric English Comments
Density 7.86 g/cc
0.284 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 187 - 223
187 - 223
annealed
293 - 321

@Treatment Temp. 538 °C
293 - 321

@Treatment Temp. 1000 °F
stress relieved
321 - 353

@Treatment Temp. 510 °C
321 - 353

@Treatment Temp. 950 °F
stress relieved
Hardness, Rockwell C 26.5

@Tempering Temp. 649 °C
26.5

@Tempering Temp. 1200 °F
39.5

@Tempering Temp. 538 °C
39.5

@Tempering Temp. 1000 °F
43.5

@Tempering Temp. 427 °C
43.5

@Tempering Temp. 800 °F
46.5

@Tempering Temp. 316 °C
46.5

@Tempering Temp. 600 °F
48.5

@Tempering Temp. 204 °C
48.5

@Tempering Temp. 400 °F
Modulus of Elasticity 207 GPa
30000 ksi
Thermal Properties Metric English Comments
CTE, linear 12.3 µm/m-°C

@Temperature 21.1 - 260 °C
6.84 µin/in-°F

@Temperature 70.0 - 500 °F
12.8 µm/m-°C

@Temperature 21.1 - 427 °C
7.10 µin/in-°F

@Temperature 70.0 - 800 °F
13.7 µm/m-°C

@Temperature 21.1 - 538 °C
7.60 µin/in-°F

@Temperature 70.0 - 1000 °F
Thermal Conductivity 3.46 W/m-K

@Temperature 93.3 °C
24.0 BTU-in/hr-ft²-°F

@Temperature 200 °F
Component Elements Properties Metric English Comments
Carbon, C 0.30 %
0.30 %
Chromium, Cr 1.7 %
1.7 %
Iron, Fe 96.35 %
96.35 %
as balance
Manganese, Mn 0.75 %
0.75 %
Molybdenum, Mo 0.40 %
0.40 %
Silicon, Si 0.50 %
0.50 %
Users viewing this material also viewed the following: