Material Notes:
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and good electrical conductivity.Typical Applications: Seals, compressors, pumps, bearingsInformation provided by SGL Carbon Group
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
Open Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
Ball Size/Load - 5/100
Modulus of Elasticity 15.2 GPa
2200 ksi
Flexural Strength 79.3 MPa
11500 psi
Compressive Strength 169 MPa
24500 psi
Thermal Properties Metric English Comments
CTE, linear 14.9 µm/m-°C

@Temperature 20.0 °C
8.30 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 3.46 W/m-K
24.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 177 °C
350 °F
In oxygen
Maximum Service Temperature, Inert 204 °C
399 °F