Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 210 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 210 W/m-K

@Temperature 20.0 - 400 °C
1460 BTU-in/hr-ft²-°F

@Temperature 68.0 - 752 °F
Hogen Duralloy H3W 68 Tungsten/32 Copper PM Metal Composite
RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is ..
Thermal Conductivity 210 - 220 W/m-K
1460 - 1530 BTU-in/hr-ft²-°F
x-y direction
MarkeTech Cu/Mo/Cu 1:4:1 Laminated Sheet
Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea..
Thermal Conductivity 210 - 220 W/m-K
1460 - 1530 BTU-in/hr-ft²-°F
x-y direction
MarkeTech Cu/Mo70-Cu30/Cu 1:4:1 Laminated Sheet
Cu/Mo/Cu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated he..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Materion Brush 1915â„¢ Annealed Temper Rod
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Materion Brush 1915â„¢ Hard Temper Rod, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Materion Brush 1915â„¢ Hard Temper Wire, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Materion Brush 1915â„¢ Hard Temper Wire, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Typical
Materion E20 Beryllium/BeO Composite, 20 Volume% BeO
Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Through Thickness
GrafTech M3 Thin Aluminum Foil Coating
Optional coating for eGRAF® SPREADERSHIELD™ graphite products. Structure: 0.127mm Al - 0.025mm PSA
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Materion AlBeMet® AM 162 HIP'd Billet, Annealed
This is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are derived by consolidating the Al/Be powder by hot isostatic pressing (HIP) ..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Materion Brush 1915â„¢ Annealed Temper Wire
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Materion Brush 1915â„¢ AT Temper Rod
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Materion Brush 1915â„¢ AT Temper Wire
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Materion Brush 1915â„¢ Hard Temper Rod, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Materion Brush 1915â„¢ Heat Treated Temper Rod, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Materion Brush 1915â„¢ Heat Treated Temper Rod, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Materion Brush 1915â„¢ Heat Treated Temper Wire, 0.050" - 0.375"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Materion Brush 1915â„¢ Heat Treated Temper Wire, 0.375" - 0.500"
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee..
Thermal Conductivity >= 210 W/m-K
>= 1460 BTU-in/hr-ft²-°F
Minimum
Materion E60 Beryllium/BeO Composite, 60 Volume% BeO
Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
ASTM E1461
M Cubed Technologies TSC-15 Titanium-alloyed Reaction Bonded Silicon Carbide
Specialty reaction-bonded SiC for applications requiring high stiffness, high toughness, and also high thermal conductivity--mechanical seals, for example Flow-through complex channels can be forme..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Ametek Molybdenum-Copper Composite AMC 6436
Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Materion AlBeMet® AM 162 Extruded Bar, Annealed
Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube..
Thermal Conductivity 210 W/m-K
1460 BTU-in/hr-ft²-°F
Materion AlBeMet® AM 162 Rolled Sheet, Annealed
Mechanical properties are typical, longitudinal values at RT. AlBeMet® AM 162 is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are..
Copyright © lookpolymers.com All Rights Reserved