Polymer Property : Thermal Conductivity = 2.22 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.220 - 0.320 W/m-K

@Temperature 100 - 250 °C
1.53 - 2.22 BTU-in/hr-ft²-°F

@Temperature 212 - 482 °F
Average value: 0.276 W/m-K Grade Count:7
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v..