Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.220 - 0.320 W/m-K @Temperature 100 - 250 °C |
1.53 - 2.22 BTU-in/hr-ft²-°F @Temperature 212 - 482 °F |
Average value: 0.276 W/m-K Grade Count:7 |
Overview of materials for Polytetrafluoroethylene (PTFE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v.. |