Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM E 1530 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 3413R PC 30% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | |
Quadrant EPP Duratron® PI D7000 PI, unfilled (ISO Data) Duratron D7000 PI – the basic grade within the Duratron PI family – is made from unfilled polyimide resin and provides maximum physical properties and best electrical and thermal insulation. Good .. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Mindel® B-322 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This mat.. |
|||
Thermal Conductivity | 0.220 - 400 W/m-K | 1.53 - 2780 BTU-in/hr-ft²-°F | Average value: 78.8 W/m-K Grade Count:12 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | DIN 52612 |
Isoflon PP Polypropylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM 1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C 177 |
SABIC Innovative Plastics Ultem 1010RV PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas r.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C 177 |
SABIC Innovative Plastics Ultem 1100EF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C 177 |
SABIC Innovative Plastics Ultem 1100EF PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM E 1530 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM E 1530 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL N110S PPE+HIPS (Europe-Africa-Middle East) NORYL N110S is an unfilled material with a Vicat B/120 of 115 ?C according ISO 306. NORYL N110S cust spec 1977 has been listed for potable water |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL PX1185 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1185 is a special NORYL grade developed for extrusion of automotive trims. NORYL PX1185 offers high heat resistance and good impact performance. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM 1000E PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. US FDA and EU Food Contact compliant. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL N110 PPE+HIPS (Europe-Africa-Middle East) NORYL N110 is an unfilled material, with a Vicat B/120 of 115 °C according ISO 306. NORYL N110 has medium temperature resistance and good |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
Westlake Plastics Zelux® 40% GF Polycarbonate 40% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | DIN 52612 |
Polyram RamTough RZ300G2 Polycarbonate, 10% Glass Fiber 10% Glass fiber reinforced polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 40.0 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 104 °F |
ISO 8302 |
Ensinger TECASINT 1011 Polyimide (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 40.0 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 104 °F |
ISO 8302 |
Ensinger TECASINT 1101 Polyimide (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Zytel® FG70G30HSR3 BK309 Nylon 66
(Unverified Data**) Information provided by DuPont Performance Polymers |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | Z direction |
Rogers Corporation 3001 Thermoplastic Chloro-Fluorocopolymer Bonding Film Rogers 3001 bonding film is a thermoplastic chloro-fluorocopolymer. It is recommended for bonding low dielectric constant PTFE (Teflon® fluorocarbon polymer) microwave stripline packages and other.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL PX1786G PPE+HIPS (Europe-Africa-Middle East) NORYL PX1786G is a 30 % glass filled material with a Vicat B/120 of 160 °C. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM 1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in natural color. Effective June, 20.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM 1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM 1000E PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer b.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM 1010M PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. |