Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 19.2 W/m-K | 133 BTU-in/hr-ft²-°F | |
Hoskins Manufacturing Chromel® Thermocouple Wire Used in Type E and Type K thermocouples. All values may vary dependent on specific design and usageChromel® is a registered trade name of Hoskins Manufacturing.Capabilities: WireRibbonSquareInsu.. |
|||
Thermal Conductivity | 19.2 W/m-K @Temperature 500 °C |
133 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Thermal Conductivity | 19.2 W/m-K @Temperature 500 °C |
133 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes 242® alloy Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Thermal Conductivity | 19.2 W/m-K @Temperature 500 °C |
133 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Thermal Conductivity | 19.2 W/m-K @Temperature 500 °C |
133 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Thermal Conductivity | 19.2 W/m-K @Temperature 500 °C |
133 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Thermal Conductivity | 19.2 W/m-K @Temperature 500 °C |
133 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Thermal Conductivity | 19.2 W/m-K @Temperature 500 °C |
133 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Thermal Conductivity | 19.2 W/m-K @Temperature 500 °C |
133 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Thermal Conductivity | 19.2 W/m-K @Temperature 500 °C |
133 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Thermal Conductivity | 19.2 W/m-K | 133 BTU-in/hr-ft²-°F | |
Special Metals MONEL® Alloy 401 A copper-nickel alloy designed for specialized electrical and electronic applications. It has a very low temperature coefficient of resistance and medium-range electrical resistivity. Used for wir.. |
|||
Thermal Conductivity | 19.1 W/m-K @Temperature 100 °C |
133 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
CMT Materials METAPOR® BF 100 AL Air Permeable Material METAPOR® is a composite material made of aluminum granules and epoxy resin. The material is air-permeable over the entire surface due to its micro-porous structure allowing for unique design consi.. |
|||
Thermal Conductivity | 19.2 W/m-K | 133 BTU-in/hr-ft²-°F | |
ATI Allegheny Ludlum AL 453™ Stainless Steel Single phase iron-chromium ferritic stainless steel alloy. Should be annealed between 1450 and 1600°F and quickly cooled. Information provided by Allegheny Ludlum |
|||
Thermal Conductivity | 19.2 W/m-K | 133 BTU-in/hr-ft²-°F | Through Plane |
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC thermosets are the most .. |