Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 19.2 W/m-K
133 BTU-in/hr-ft²-°F
Hoskins Manufacturing Chromel® Thermocouple Wire
Used in Type E and Type K thermocouples. All values may vary dependent on specific design and usageChromel® is a registered trade name of Hoskins Manufacturing.Capabilities: WireRibbonSquareInsu..
Thermal Conductivity 19.2 W/m-K

@Temperature 500 °C
133 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes 242® alloy, cold reduced sheet, annealed, 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 19.2 W/m-K

@Temperature 500 °C
133 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes 242® alloy
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 19.2 W/m-K

@Temperature 500 °C
133 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 19.2 W/m-K

@Temperature 500 °C
133 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 19.2 W/m-K

@Temperature 500 °C
133 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 19.2 W/m-K

@Temperature 500 °C
133 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes 242® alloy, cold reduced sheet, annealed
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 19.2 W/m-K

@Temperature 500 °C
133 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes 242® alloy, cold reduced sheet, annealed and 20% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 19.2 W/m-K

@Temperature 500 °C
133 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 19.2 W/m-K

@Temperature 500 °C
133 BTU-in/hr-ft²-°F

@Temperature 932 °F
Haynes 242® alloy, cold reduced sheet, annealed and aged
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Thermal Conductivity 19.2 W/m-K
133 BTU-in/hr-ft²-°F
Special Metals MONEL® Alloy 401
A copper-nickel alloy designed for specialized electrical and electronic applications. It has a very low temperature coefficient of resistance and medium-range electrical resistivity. Used for wir..
Thermal Conductivity 19.2 W/m-K
133 BTU-in/hr-ft²-°F
ATI Allegheny Ludlum AL 453™ Stainless Steel
Single phase iron-chromium ferritic stainless steel alloy. Should be annealed between 1450 and 1600°F and quickly cooled. Information provided by Allegheny Ludlum
Thermal Conductivity 19.2 W/m-K
133 BTU-in/hr-ft²-°F
Through Plane
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material
Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC thermosets are the most ..