Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 19.1 W/m-K @Temperature 100 °C |
133 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
CMT Materials METAPOR® BF 100 AL Air Permeable Material METAPOR® is a composite material made of aluminum granules and epoxy resin. The material is air-permeable over the entire surface due to its micro-porous structure allowing for unique design consi.. |