Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 1180 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 140 - 170 W/m-K
972 - 1180 BTU-in/hr-ft²-°F
MarkeTech AN 160 Aluminum Nitride Ceramic Substrate, 99% Purity
Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µ..
Thermal Conductivity 165 - 170 W/m-K
1150 - 1180 BTU-in/hr-ft²-°F
z direction
MarkeTech Cu/Mo/Cu 1:5:1 Laminated Sheet
Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea..
Thermal Conductivity 160 - 170 W/m-K
1110 - 1180 BTU-in/hr-ft²-°F
z direction
MarkeTech Cu/Mo/Cu 13:74:13 Laminated Sheet
Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea..
Thermal Conductivity 150 - 170 W/m-K
1040 - 1180 BTU-in/hr-ft²-°F
Temper T651
Constellium PLAN 6061 Aluminum Rolled Plate
Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
Thermal Conductivity 150 - 170 W/m-K
1040 - 1180 BTU-in/hr-ft²-°F
Temper T651
Constellium PLAN 6082 Aluminum Rolled Plate
Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
Thermal Conductivity 150 - 170 W/m-K
1040 - 1180 BTU-in/hr-ft²-°F
temper T651
Constellium Planoxal® 60 Aluminum plate
The advantage of Planoxal®-60 plates over other standard EN AW-6082 alloy products is their low level of internal stress. They are also suitable for technical anodizing. Planoxal®-60 is mainly use..
Thermal Conductivity 150 - 170 W/m-K
1040 - 1180 BTU-in/hr-ft²-°F
Temper T651
Constellium ALPLAN® 6061 Rolled Precision Aluminum Plate, Milled Both Sides
Precision plates in ALPLAN® 6061 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta..
Thermal Conductivity 150 - 170 W/m-K
1040 - 1180 BTU-in/hr-ft²-°F
Temper T651
Constellium ALPLAN® 6082 Rolled Precision Aluminum Plate, Milled Both Sides
Precision plates in ALPLAN® 6082 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta..