Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.282 - 0.513 W/m-K
1.96 - 3.56 BTU-in/hr-ft²-°F
Average value: 0.407 W/m-K Grade Count:4
Overview of materials for Phenolic, Ablative Coating
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Ablative Coating". Each property range of values reported is minimum and maximum values of app..
Thermal Conductivity 0.282 W/m-K
1.96 BTU-in/hr-ft²-°F
Haveg 41NA Phenolic; Silicate Filled
A proprietary thermoset plastic consisting of a phenol-formaldehyde resin and non-asbestos silicate fillers.