Overview of materials for Phenolic, Ablative Coating

Category Polymer , Thermoset , Phenolic , Phenolic, Ablative Coating
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Phenolic, Ablative Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Ablative Coating". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.25 - 1.85 g/cc
0.0452 - 0.0668 lb/in³
Average value: 1.53 g/cc Grade Count:4
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4.30 - 40.4 MPa
624 - 5860 psi
Average value: 21.8 MPa Grade Count:4
Elongation at Break 0.660 - 12.5 %
0.660 - 12.5 %
Average value: 6.60 % Grade Count:4
Thermal Properties Metric English Comments
Thermal Conductivity 0.282 - 0.513 W/m-K
1.96 - 3.56 BTU-in/hr-ft²-°F
Average value: 0.407 W/m-K Grade Count:4