Material Notes:
A proprietary thermoset plastic consisting of a phenol-formaldehyde resin and non-asbestos silicate fillers.
Physical Properties Metric English Comments
Density 1.72 g/cc
0.0621 lb/in³
Mechanical Properties Metric English Comments
Hardness, Barcol 64
64
Tensile Strength, Ultimate 38.0 MPa
5510 psi
Elongation at Break 0.66 %
0.66 %
Tensile Modulus 9.45 GPa
1370 ksi
Flexural Yield Strength 67.8 MPa
9830 psi
Compressive Yield Strength 133 MPa
19300 psi
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C

@Temperature 20.0 °C
8.33 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
Thermal Conductivity 0.282 W/m-K
1.96 BTU-in/hr-ft²-°F