Polymer Property : Thermal Conductivity = 1.83 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.263 W/m-K
1.83 BTU-in/hr-ft²-°F
Arlon IsoClad 917 Non-Woven Fiberglass Reinforced PTFE
Traditional - Highest Performance, PTFE Coated Light Woven Glass Styles, Interdispersed PTFE FilmInformation provided by Arlon Materials for Electronics (MED).
Thermal Conductivity 0.263 W/m-K
1.83 BTU-in/hr-ft²-°F
Arlon IsoClad 933 Non-Woven Fiberglass Reinforced PTFE
Traditional - Highest Performance, PTFE Coated Light Woven Glass Styles, Interdispersed PTFE FilmInformation provided by Arlon Materials for Electronics (MED).
Thermal Conductivity 0.264 W/m-K
1.83 BTU-in/hr-ft²-°F
Melt
BASF Ultramid® 8202 HS PA6 (Conditioned)
Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab..
Thermal Conductivity 0.264 W/m-K
1.83 BTU-in/hr-ft²-°F
Melt
BASF Ultramid® 8202 HS PA6 (Dry)
Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab..
Thermal Conductivity 0.264 W/m-K
1.83 BTU-in/hr-ft²-°F
Melt
BASF Ultramid® 8202 PA6 (Conditioned)
Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult..
Thermal Conductivity 0.264 W/m-K
1.83 BTU-in/hr-ft²-°F
Melt
BASF Ultramid® 8202 PA6 (Dry)
Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult..