Arlon IsoClad 917 Non-Woven Fiberglass Reinforced PTFE

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Arlon
Trade Name IsoClad
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon IsoClad 917 Non-Woven Fiberglass Reinforced PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Traditional - Highest Performance, PTFE Coated Light Woven Glass Styles, Interdispersed PTFE FilmInformation provided by Arlon Materials for Electronics (MED).
Physical Properties Metric English Comments
Density 2.23 g/cc
0.0806 lb/in³
Water Absorption 0.040 %
0.040 %
Outgassing - Total Mass Loss 0.00 %
0.00 %
Collected Volatile
0.020 %
0.020 %
Total Mass Loss
Mechanical Properties Metric English Comments
Peel Strength 1.75 kN/m
10.0 pli
Thermal Properties Metric English Comments
CTE, linear 46.0 µm/m-°C
25.6 µin/in-°F
x direction
47.0 µm/m-°C
26.1 µin/in-°F
y direction
CTE, linear, Transverse to Flow 236 µm/m-°C
131 µin/in-°F
z direction
Thermal Conductivity 0.263 W/m-K
1.83 BTU-in/hr-ft²-°F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 2.17

@Frequency 1.00e+10 Hz
2.17

@Frequency 1.00e+10 Hz
2.17

@Thickness 0.127 mm
2.17

@Thickness 0.00500 in
2.17

@Thickness 1.57 mm
2.17

@Thickness 0.0620 in
Dissipation Factor 0.0013

@Frequency 1.00e+10 Hz
0.0013

@Frequency 1.00e+10 Hz
Descriptive Properties Value Comments
Temperature Coefficient of Dielectric (ppm/°C) -157