Polymer Property : Thermal Conductivity = 0.390 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.390 W/m-K

@Temperature 100 °C
2.71 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Plenco 2000 Phenolic, Granular, Compression Molded
PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo..
Thermal Conductivity 0.390 W/m-K
2.71 BTU-in/hr-ft²-°F
ASTM C 177
Adamas Adalon® 301 PTFE, 10% Graphite
Information provided by Adamas, HPM
Thermal Conductivity 0.390 W/m-K
2.71 BTU-in/hr-ft²-°F
ASTM C 177
Adamas Adalon® 826 PTFE, 50% Stainless steel
Information provided by Adamas, HPM
Thermal Conductivity 0.390 W/m-K
2.71 BTU-in/hr-ft²-°F
Mfr. internal test
Ascend Performance Materials VYDYNE® R400G Nylon, Mineral and Glass Reinforced
Typical property data. VYDYNE is a registered trademark of Solutia Inc.
Thermal Conductivity 0.390 W/m-K
2.71 BTU-in/hr-ft²-°F
DIN 52612
Lehmann & Voss LUVOCOM® 1-7003 Polyamide 66, with carbon fiber and PTFE, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Thermal Conductivity 0.390 W/m-K
2.71 BTU-in/hr-ft²-°F
Sorbothane Polyurethane Damping Material, 70 Durometer
Sorbothane® is a thermoset, polyether-based polyurethane viscoelastic material that combines high energy absorption with faultless memory. Sorbothane turns mechanical energy into heat. As the mat..
Thermal Conductivity 0.390 W/m-K
2.71 BTU-in/hr-ft²-°F
Quadrant EPP Duratron® PI D7015G PI, bearing grade (ISO Data)
This grade contains 15 % graphite, added to provide long wear and low friction Good performance at elevated temperature (>425 °C) Good chemical resistance Easily machined from a broad range of shap..