Adamas Adalon® 826 PTFE, 50% Stainless steel

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Adamas
Trade Name Adalon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adamas Adalon® 826 PTFE, 50% Stainless steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Adamas, HPM
Physical Properties Metric English Comments
Specific Gravity 3.30 - 3.35 g/cc
3.30 - 3.35 g/cc
ASTM D792
Deformation 6.0 - 7.5 %
6.0 - 7.5 %
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 60 - 65
60 - 65
ASTM D2240
Ball Indentation Hardness 40.0 - 44.0 MPa
5800 - 6380 psi
ISO 2032
Tensile Strength at Break >= 18.0 MPa
>= 2610 psi
ASTM D4894
Elongation at Break >= 180 %
>= 180 %
ASTM D4894
Tensile Modulus 1.66 GPa
241 ksi
ASTM D638
Coefficient of Friction, Dynamic 0.41 - 0.43
0.41 - 0.43
ASTM D1894
Coefficient of Friction, Static 0.44 - 0.46
0.44 - 0.46
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear 82.8 µm/m-°C
46.0 µin/in-°F
ASTM D696
Thermal Conductivity 0.390 W/m-K
2.71 BTU-in/hr-ft²-°F
ASTM C 177
Melting Point 327 °C
621 °F
DSC
Maximum Service Temperature, Air 260 °C
500 °F
DSC
Minimum Service Temperature, Air -80.0 °C
-112 °F
DSC
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
Surface Resistance 1000 ohm
1000 ohm
ASTM D257