Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0407 W/m-K | 0.282 BTU-in/hr-ft²-°F | 15g/L; KS M 3808 |
LG Chemical B160 EPS, Non-Flame Retardant Feature: Expendable Polystyrene, Non-Flame RetardantApplication: Package, Fruit/Fish Box, Floats, Pad, Ice BoxCAS No. 9003-53-6 and 109-66-0Information provided by LG Chemical |
|||
Thermal Conductivity | 0.0407 W/m-K | 0.282 BTU-in/hr-ft²-°F | 15g/L; KS M 3808 |
LG Chemical B240 EPS, Non-Flame Retardant Feature: Expendable Polystyrene, Non-Flame RetardantApplication: Package, Fruit/Fish Box, Floats, Pad, Ice BoxCAS No. 9003-53-6 and 109-66-0Information provided by LG Chemical |
|||
Thermal Conductivity | 0.0407 W/m-K | 0.282 BTU-in/hr-ft²-°F | 15g/L; KS M 3808 |
LG Chemical R160 EPS, Flame Retardant Feature: Expendable Polystyrene, Flame RetardantApplication: Insulation Board, Sandwich Panel Civil Engineering & Construction MaterialsCAS No. 9003-53-6, 109-66-0, 3194-55-6 and 106-97-8Information.. |
|||
Thermal Conductivity | 0.0407 W/m-K | 0.282 BTU-in/hr-ft²-°F | 15g/L; KS M 3808 |
LG Chemical R240 EPS, Flame Retardant Feature: Expendable Polystyrene, Flame RetardantApplication: Insulation Board, Sandwich Panel Civil Engineering & Construction MaterialsCAS No. 9003-53-6, 109-66-0, 3194-55-6 and 106-97-8Information.. |
|||
Thermal Conductivity | 0.0407 W/m-K | 0.282 BTU-in/hr-ft²-°F | mean temp of 83°C; ISO 8301 |
Zotefoams ZOTEK® F 40 HT LS PVDF Foam Zotek® F 40 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |
|||
Thermal Conductivity | 0.0407 W/m-K | 0.282 BTU-in/hr-ft²-°F | mean temp of 83°C; ISO 8301 |
Zotefoams ZOTEK® F OSU Semi-Rigid PVDF Foam Zotek® F OSU is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and .. |