LG Chemical R240 EPS, Flame Retardant

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical R240 EPS, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Feature: Expendable Polystyrene, Flame RetardantApplication: Insulation Board, Sandwich Panel Civil Engineering & Construction MaterialsCAS No. 9003-53-6, 109-66-0, 3194-55-6 and 106-97-8Information provided by LG Chemical
Physical Properties Metric English Comments
Water Absorption 0.42 %
0.42 %
[g/100cm<sup>2</sup>], 30g/L; KS M 3808
0.45 %
0.45 %
[g/100cm<sup>2</sup>], 25g/L; KS M 3808
0.72 %
0.72 %
[g/100cm<sup>2</sup>], 20g/L; KS M 3808
0.75 %
0.75 %
[g/100cm<sup>2</sup>], 15g/L; KS M 3808
Mechanical Properties Metric English Comments
Flexural Yield Strength 0.176 MPa
25.5 psi
15g/L; KS M 3808
0.260 MPa
37.7 psi
20g/L; KS M 3808
0.337 MPa
48.9 psi
25g/L; KS M 3808
0.414 MPa
60.0 psi
30g/L; KS M 3808
Impact 0.86
0.86
[kg/cm<sup>2<sup>], 15g/L; KS M 3808
1.26
1.26
[kg/cm<sup>2<sup>], 20g/L; KS M 3808
1.75
1.75
[kg/cm<sup>2<sup>], 25g/L; KS M 3808
2.15
2.15
[kg/cm<sup>2<sup>], 30g/L; KS M 3808
Thermal Properties Metric English Comments
Thermal Conductivity 0.0337 W/m-K
0.234 BTU-in/hr-ft²-°F
30g/L; KS M 3808
0.0360 W/m-K
0.250 BTU-in/hr-ft²-°F
25g/L; KS M 3808
0.0372 W/m-K
0.258 BTU-in/hr-ft²-°F
20g/L; KS M 3808
0.0407 W/m-K
0.282 BTU-in/hr-ft²-°F
15g/L; KS M 3808