Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zotefoams ZOTEK® F 40 HT LS PVDF Foam

Category Polymer , Thermoplastic , Fluoropolymer , PVDF
Manufacturer Zotefoams
Trade Name ZOTEK®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zotefoams ZOTEK® F 40 HT LS PVDF Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zotek® F 40 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.This grade is recommended for applications where very low smoke is required in the event of a fire.Compliant with US FDA regulations.Information provided by Zotefoams
Physical Properties Metric English Comments
Density 0.0340 g/cc
0.00123 lb/in³
ISO 845
Cell Length 0.180 mm
0.00709 in
Mechanical Properties Metric English Comments
Tensile Strength 0.544 MPa
78.9 psi
ISO 1798
Elongation at Break 129 %
129 %
Compressive Yield Strength 0.0920 MPa

@Strain 25.0 %
13.3 psi

@Strain 25.0 %
ISO 7214
Tear Strength 0.823 kN/m
4.70 pli
ISO 8067
Compression Set 29 %

@Time 79200 sec,
Strain 50.0 %
29 %

@Time 22.0 hour,
Strain 50.0 %
0.5 hr recovery; ASTM D3575
Thermal Properties Metric English Comments
Thermal Conductivity 0.0321 W/m-K
0.223 BTU-in/hr-ft²-°F
mean temp of 0°C; ISO 8301
0.0370 W/m-K
0.257 BTU-in/hr-ft²-°F
mean temp of 50°C; ISO 8301
0.0407 W/m-K
0.282 BTU-in/hr-ft²-°F
mean temp of 83°C; ISO 8301
Maximum Service Temperature, Air 155 °C
311 °F
Flammability Test 0.00

@Thickness 3.00 mm
0.00

@Thickness 0.118 in
Smoke Developed Index; ASTM E84/UL 723
5.0

@Thickness 25.0 mm
5.0

@Thickness 0.984 in
Smoke Developed Index; ASTM E84/UL 723
Flame Spread Index 0.00

@Thickness 3.00 mm
0.00

@Thickness 0.118 in
ASTM E84/UL 723
5.0

@Thickness 25.0 mm
5.0

@Thickness 0.984 in
ASTM E84/UL 723
Descriptive Properties Value Comments
Flammability Heat Release: FAR/CS 25.853, 2 min total
30.2 kWmin/m<sup>2</sup>
Heat Release: FAR/CS 25.853, Peak
35 kW/m<sup>2</sup>
Smoke Emission: ABD0031
8 Ds Max in 4 min, flaming
Smoke Emission: ABD0031
7 Ds Max in 4 min, not flaming
Smoke Emission: FAR/JAR/CS 25.853
8 Ds Max in 4 min, flaming
Toxic Gas Emission: ABD0031
Pass at 25 mm
Users viewing this material also viewed the following: