Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.206 - 0.245 W/m-K | 1.43 - 1.70 BTU-in/hr-ft²-°F | Average value: 0.238 W/m-K Grade Count:6 |
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Thermal Conductivity | 0.231 - 0.245 W/m-K | 1.60 - 1.70 BTU-in/hr-ft²-°F | Average value: 0.238 W/m-K Grade Count:4 |
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu.. |