Thermal Properties Metric English Comments
Thermal Conductivity 0.0570 W/m-K

@Temperature 200 °C
0.396 BTU-in/hr-ft²-°F

@Temperature 392 °F
Sharadaa Ceramics Calcium Silicate Block
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Thermal Conductivity 0.0570 W/m-K
0.396 BTU-in/hr-ft²-°F
Liquid
3M Fluorinert™ FC-72 Electronic Liquid
3M™ Fluorinert™ Liquid FC-72 is a non-conductive, thermally and chemically stable liquid ideal for many direct contact single and two phase low temperature heat transfer applications, in testing, ..
Thermal Conductivity 0.0570 W/m-K

@Temperature 40.0 °C
0.396 BTU-in/hr-ft²-°F

@Temperature 104 °F
3M Novec™ 649 Engineered Fluid
3M™ Novec™ 649 Engineered Fluid is a clear, colorless and low odor fluid, one in a line of 3M products designed as replacements for ozone depleting substances (ODSs) and compounds with high global..