Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Novec™ 649 Engineered Fluid

Category Fluid
Manufacturer 3M
Trade Name Novec™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Novec™ 649 Engineered Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Novec™ 649 Engineered Fluid is a clear, colorless and low odor fluid, one in a line of 3M products designed as replacements for ozone depleting substances (ODSs) and compounds with high global warming potentials (GWPs) such as sulfur hexafluoride (SF6) and hydrofluorocarbons (HFCs), such as HFC-134a and HFC 245fa. 3M Novec 649 Engineered Fluid is an advanced heat transfer fluid, balancing customer needs for physical, thermal and electrical properties, with desirable environmental properties.Typical Applications Novec 649 fluid is an effective heat transfer fluid with a boiling point of 49ºC. Novec 649 fluid is useful in heat transfer particularly where non-flammability or environmental factors are a consideration. Examples of systems which benefit from use Novec 649 fluid include:Electronics Cooling (Single or Dual Phase): Power Electronics such as IGBTs or invertersTransformers and other equipment (SF6 replacement) Computer/Data Center CoolingOrganic Rankine Cycle: Diesel EnginesGeneratorsGeothermal ApplicationsSolar ApplicationsInformation provided by 3M
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
Liquid
1.56 g/cc

@Temperature 40.0 °C
0.0564 lb/in³

@Temperature 104 °F
1.79 g/cc

@Temperature -40.0 °C
0.0647 lb/in³

@Temperature -40.0 °F
1.96 g/cc

@Temperature -100 °C
0.0708 lb/in³

@Temperature -148 °F
Viscosity 0.64 cP
0.64 cP
Absolute
Kinematic Viscosity 0.40 cSt
0.40 cSt
Viscosity Measure 0.35 cSt

@Temperature 30.0 °C
0.35 cSt

@Temperature 86.0 °F
0.60 cSt

@Temperature -10.0 °C
0.60 cSt

@Temperature 14.0 °F
1.75 cSt

@Temperature -60.0 °C
1.75 cSt

@Temperature -76.0 °F
20 cSt

@Temperature -105 °C
20 cSt

@Temperature -157 °F
Molecular Weight 316 g/mol
316 g/mol
Vapor Pressure 0.400 bar
300 torr
Surface Tension 10.8 dynes/cm
10.8 dynes/cm
Thermal Properties Metric English Comments
Heat of Vaporization 88.0 J/g
37.9 BTU/lb
CTE, linear 1800 µm/m-°C
1000 µin/in-°F
Specific Heat Capacity 1.103 J/g-°C
0.2636 BTU/lb-°F
Thermal Conductivity 0.0590 W/m-K
0.409 BTU-in/hr-ft²-°F
0.0570 W/m-K

@Temperature 40.0 °C
0.396 BTU-in/hr-ft²-°F

@Temperature 104 °F
0.0710 W/m-K

@Temperature -40.0 °C
0.493 BTU-in/hr-ft²-°F

@Temperature -40.0 °F
0.0820 W/m-K

@Temperature -100 °C
0.569 BTU-in/hr-ft²-°F

@Temperature -148 °F
Boiling Point 49.0 °C
120 °F
Pour Point -108 °C
-162 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
Dielectric Constant 1.8

@Frequency 1000 Hz
1.8

@Frequency 1000 Hz
Dielectric Strength >= 1.57 kV/mm
>= 40.0 kV/in
0.1" gap
Chemical Properties Metric English Comments
Critical Pressure 18.8 bar
14100 torr
Critical Temperature 169 °C
336 °F
Users viewing this material also viewed the following: