Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 860 µm/m-°C @Temperature 25.0 - 100 °C |
478 µin/in-°F @Temperature 77.0 - 212 °F |
|
ExxonMobil Exxon Hyjet IV-A Exxon HyJet IV-Aplus is a fire-resistant phosphate ester hydraulic fluid designed for use in commercial aircraft. It is the best-performing Type IV fluid and offers to a great extent many of the per.. |
|||
CTE, linear | 860 µm/m-°C @Temperature 25.0 - 100 °C |
478 µin/in-°F @Temperature 77.0 - 212 °F |
|
ExxonMobil Exxon Hyjet V Exxon HyJet V is a Type V fire-resistant phosphate ester hydraulic fluid, which is superior in thermal and hydrolytic stability to commercially available Type IV hydraulic fluids. Better stability m.. |
|||
CTE, linear | 860 µm/m-°C @Temperature 25.0 - 100 °C |
478 µin/in-°F @Temperature 77.0 - 212 °F |
|
ExxonMobil Exxon Hyjet IV-A Exxon HyJet IV-Aplus is a fire-resistant phosphate ester hydraulic fluid designed for use in commercial aircraft. It is the best-performing Type IV fluid and offers to a great extent many of the per.. |
|||
CTE, linear | 860 µm/m-°C @Temperature 25.0 - 100 °C |
478 µin/in-°F @Temperature 77.0 - 212 °F |
|
ExxonMobil Exxon Hyjet V Exxon HyJet V is a Type V fire-resistant phosphate ester hydraulic fluid, which is superior in thermal and hydrolytic stability to commercially available Type IV hydraulic fluids. Better stability m.. |