Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 21.0 - 82.0 µm/m-°C @Temperature 40.0 - 130 °C |
11.7 - 45.6 µin/in-°F @Temperature 104 - 266 °F |
Average value: 50.5 µm/m-°C Grade Count:19 |
Overview of materials for Phenolic, Novolac, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values.. |
|||
CTE, linear | 17.0 - 82.0 µm/m-°C | 9.44 - 45.6 µin/in-°F | Average value: 45.3 µm/m-°C Grade Count:22 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
CTE, linear | 70.0 - 82.0 µm/m-°C | 38.9 - 45.6 µin/in-°F | |
Master Bond FLM36 B-staged film for high performance bonding and sealing Master Bond FLM36 is a film adhesive with exceptional strength properties, high temperature resistance and first class thermal conductivity and electrical insulation properties. Based on the Master .. |