Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 14.8 µm/m-°C @Temperature 25.0 - 500 °C |
8.22 µin/in-°F @Temperature 77.0 - 932 °F |
|
Wieland Simidur S 1S PFM Alloy Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental |
|||
CTE, linear | 14.8 µm/m-°C @Temperature 20.0 - 1000 °C |
8.22 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Ceradyne Ceralloy® 6705 MgO-SiC Applications: absorbersbuttonsInformation provided by Ceradyne Company |