Wieland Simidur S 1S PFM Alloy

Category Metal , Nonferrous Metal , Precious Metal , Palladium Alloy
Manufacturer Wieland
Trade Name Simidur
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wieland Simidur S 1S PFM Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental
Physical Properties Metric English Comments
Density 11.3 g/cc
0.408 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 270
270
HV5/30; after porcelain firing
280
280
HV5/30; hardened
Tensile Strength, Yield 560 MPa

@Strain 0.200 %
81200 psi

@Strain 0.200 %
after porcelain firing
600 MPa

@Strain 0.200 %
87000 psi

@Strain 0.200 %
hardened
Elongation at Break 6.0 %
6.0 %
hardened
9.0 %
9.0 %
after porcelain firing
Modulus of Elasticity 126 GPa
18300 ksi
Thermal Properties Metric English Comments
CTE, linear 14.8 µm/m-°C

@Temperature 25.0 - 500 °C
8.22 µin/in-°F

@Temperature 77.0 - 932 °F
Component Elements Properties Metric English Comments
Gallium, Ga 2.0 %
2.0 %
Indium, In 1.0 %
1.0 %
Palladium, Pd 56 %
56 %
Ruthenium, Ru <= 0.10 %
<= 0.10 %
Silver, Ag 32 %
32 %
Tin, Sn 9.0 %
9.0 %
Processing Properties Metric English Comments
Processing Temperature 849 °C
1560 °F
Preheating Temp.
Melt Temperature 1080 - 1200 °C
1980 - 2190 °F
Casting Temperature 1350 °C
2460 °F
Descriptive Properties Value Comments
Color white