Thermal Properties Metric English Comments
CTE, linear 14.8 µm/m-°C

@Temperature 25.0 - 500 °C
8.22 µin/in-°F

@Temperature 77.0 - 932 °F
Wieland Simidur S 1S PFM Alloy
Palladium-base ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental
CTE, linear 14.8 µm/m-°C

@Temperature 20.0 - 1000 °C
8.22 µin/in-°F

@Temperature 68.0 - 1830 °F
Ceradyne Ceralloy® 6705 MgO-SiC
Applications: absorbersbuttonsInformation provided by Ceradyne Company