Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 53.8 µm/m-°C | 29.9 µin/in-°F | ASTM E831 |
KYDEX® 2200LT Thermoplastic Sheet for Mass Transit Applications Features:Meets flamespread and smoke development requirements listed in 49 CFR 238Excellent formability and fabrication characteristicsAllows for tight tolerance controlsExcellent resistance to graf.. |
|||
CTE, linear | 53.8 µm/m-°C @Temperature -30.0 - 30.0 °C |
29.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D-3386 |
CMT Materials REN Shape® 460 Prototype Tool & Precision Modeling Board REN Shape 460 is a moderate density precision modeling board that features a lower coefficient of thermal expansion to provide enhanced dimensional stability over a broader temperature range than ot.. |