Material Notes:
Features:Meets flamespread and smoke development requirements listed in 49 CFR 238Excellent formability and fabrication characteristicsAllows for tight tolerance controlsExcellent resistance to graffiti, chemicals and stainingSuggested Applications:SeatbacksArmrestsWindow ShroudsBulkhead ComponentsWall and Ceiling PanelsInformation provided by Kydex, LLC.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength 52.7 MPa
7640 psi
ASTM D638
Tensile Modulus 3.895 GPa
564.9 ksi
ASTM D638
Flexural Strength 77.9 MPa
11300 psi
ASTM D790
Flexural Modulus 3.11 GPa
451 ksi
ASTM D790
Izod Impact, Notched 1.40 J/cm
2.62 ft-lb/in
ASTM D256
Gardner Impact 14.2 J

@Temperature -29.0 °C
10.5 ft-lb

@Temperature -20.2 °F
ASTM D5420
40.9 J

@Temperature 22.0 °C
30.2 ft-lb

@Temperature 71.6 °F
ASTM D5420
Thermal Properties Metric English Comments
CTE, linear 53.8 µm/m-°C
29.9 µin/in-°F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 89.0 °C
192 °F
ASTM D648
Flame Spread Index <= 35
<= 35
I<sub>S</sub> value; No burning drip; ASTM E162
Smoke Density <= 100 min
<= 100 min
D<sub>S</sub>(1.5); ASTM E662
<= 200 min
<= 200 min
D<sub>S</sub>(4.0); ASTM E662
Descriptive Properties Value Comments
Toxic Gas Generation Pass
Bombardier; SMP 800-C
Pass
Boeing; BSS 7239