Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 27.0 - 93.6 µm/m-°C | 15.0 - 52.0 µin/in-°F | Average value: 70.3 µm/m-°C Grade Count:12 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
CTE, linear | 93.6 - 93.6 µm/m-°C @Temperature 0.000 - 100 °C |
52.0 - 52.0 µin/in-°F @Temperature 32.0 - 212 °F |
Average value: 93.6 µm/m-°C Grade Count:3 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
CTE, linear | 72.0 - 93.6 µm/m-°C @Temperature 0.000 - 156 °C |
40.0 - 52.0 µin/in-°F @Temperature 32.0 - 312 °F |
Average value: 78.6 µm/m-°C Grade Count:6 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |