Polymer Property : CTE, linear = 5.44 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 9.80 µm/m-°C

@Temperature 20.0 °C
5.44 µin/in-°F

@Temperature 68.0 °F
Hogen Duralloy H20TC 70 Tungsten Carbide/30 Copper PM Metal Composite
Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Extremely hard and wear resistant t..
CTE, linear 9.80 µm/m-°C

@Temperature 260 °C
5.44 µin/in-°F

@Temperature 500 °F
Ferro IP 510 Thick Film Glass
Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto..
CTE, linear 9.80 µm/m-°C

@Temperature 25.0 - 700 °C
5.44 µin/in-°F

@Temperature 77.0 - 1290 °F
Du-Co Ceramics S-570 Silica
Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu..
CTE, linear 9.80 µm/m-°C

@Temperature 20.0 °C
5.44 µin/in-°F

@Temperature 68.0 °F
California Fine Wire Alloy 52 Nickel Iron Alloy
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
CTE, linear 9.80 µm/m-°C

@Temperature 20.0 - 150 °C
5.44 µin/in-°F

@Temperature 68.0 - 302 °F
ATI Allegheny Ludlum AL 4466™ Ferritic Stainless Steel
Low carbon, low nitrogen ferritic stainless steel alloy. Characteristics:outstanding resistance to chloride pitting and crevice corrosion, improved resistance over austenitic stainless steels to ch..