Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 9.80 µm/m-°C @Temperature 20.0 °C |
5.44 µin/in-°F @Temperature 68.0 °F |
|
Hogen Duralloy H20TC 70 Tungsten Carbide/30 Copper PM Metal Composite Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Extremely hard and wear resistant t.. |
|||
CTE, linear | 9.80 µm/m-°C @Temperature 260 °C |
5.44 µin/in-°F @Temperature 500 °F |
|
Ferro IP 510 Thick Film Glass Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto.. |
|||
CTE, linear | 9.80 µm/m-°C @Temperature 25.0 - 700 °C |
5.44 µin/in-°F @Temperature 77.0 - 1290 °F |
|
Du-Co Ceramics S-570 Silica Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu.. |
|||
CTE, linear | 9.80 µm/m-°C @Temperature 20.0 °C |
5.44 µin/in-°F @Temperature 68.0 °F |
|
California Fine Wire Alloy 52 Nickel Iron Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
CTE, linear | 9.80 µm/m-°C @Temperature 20.0 - 150 °C |
5.44 µin/in-°F @Temperature 68.0 - 302 °F |
|
ATI Allegheny Ludlum AL 4466™ Ferritic Stainless Steel Low carbon, low nitrogen ferritic stainless steel alloy. Characteristics:outstanding resistance to chloride pitting and crevice corrosion, improved resistance over austenitic stainless steels to ch.. |